MATERIALS

 

Comparison table according to different standards for the most frequently used steels
Basic material
Quarto plates 8-60×2000 (2500) x6000 mm (thickness 65-130 mm upon request)
Round bars Ø20-Ø400mm (bigger Ø upon request)
Thick-wall pipes Ø100-Ø250mm

STEEL GRADEW.Nr.EN DESIGNATIONAISI/ASTM DESIGNATIONUNS DESIGNATION%C %Si %Mn%P%S%Cr%Ni%Mo%Ti%Cu%NCHARACTERISTIC
AUSTENITIC1.4301X5CrNi18-10304S30400≤0,07≤1,00≤2,00≤0,045≤0,01517,5-19,58,00-10,5///≤0,10Good corrosion resistance
AUSTENITIC1.4306X2CrNi19-11304LS30403≤0,03≤1,00≤2,00≤0,045≤0,01518,0-20,010,0-12,0///≤0,10Good corrosion resistance
AUSTENITIC1.4307X2CrNi18-9304LS30403≤0,03≤1,00≤2,00≤0,045≤0,01518,0-20,010,0-12,0///≤0,10Good corrosion resistance
AUSTENITIC1.4541X6CrNiTi18-10321S32100≤0,08≤1,00≤2,00≤0,045≤0,01517,0-19,09,00-12,0/5xC to 0,70//Good corrosion resistance
AUSTENITIC HEAT-RESISTANT 1.4878X8CrNiTi18-10321HS32109≤0,10≤1,00≤2,00≤0,045≤0,01517,0-19,09,00-12,0/5xC to 0,70//High Temperature Resistance
AUSTENITIC HEAT-RESISTANT 1.4828X15CrNiSi20-12309S30900≤0,201,50-2,50≤2,00≤0,045≤0,01519,0-21,011,0-13,0///≤0,10High Temperature Resistance
AUSTENITIC HEAT-RESISTANT 1.4841X15CrNiSi25-21314S31400≤0,201,50-2,50≤2,00≤0,045≤0,01524,0-26,019,0-22,0///≤0,10High Temperature Resistance
AUSTENITIC WITH HIGH Nickel & Molybdenum1.4539X1NiCrMoCu25-20-5904LN08904≤0,20≤0,70≤2,00≤0,030≤0,01019,0-21,024,0-26,04,00-5,00/1,20-2,00≤0,15High Temperature Resistance
AUSTENITIC WITH Molybdenum1.4401X5CrNiMo17-12-2316S31600≤0,07≤1,00≤2,00≤0,045≤0,01516,5-18,510,0-13,02,00-2,50//≤0,10Extreme corrosion resistance
AUSTENITIC WITH Molybdenum1.4436X3CrNiMo17-13-3316S31600≤0,05≤1,00≤2,00≤0,045≤0,01516,5-18,510,5-13,02,50-3,00//≤0,10Extreme corrosion resistance
AUSTENITIC WITH Molybdenum1.4432X2CrNiMo17-12-3316LS31603≤0,03≤1,00≤2,00≤0,045≤0,01516,5-18,510,5-13,02,50-3,00//≤0,10Extreme corrosion resistance
AUSTENITIC WITH Molybdenum1.4404X2CrNiMo17-12-2316LS31603≤0,03≤1,00≤2,00≤0,045≤0,01516,5-18,510,0-13,02,00-2,50//≤0,10Extreme corrosion resistance
AUSTENITIC WITH Molybdenum1.4435X2CrNiMo18-14-3316LS31603≤0,03≤1,00≤2,00≤0,045≤0,01517,0-19,012,5-15,02,50-3,00//≤0,10Extreme corrosion resistance
AUSTENITIC WITH Molybdenum1.4571X6CrNiMoTi17-12-2316TiS31635≤0,08≤1,00≤2,00≤0,045≤0,01516,5-18,510,5-13,52,00-2,505xC to 0,70//Extreme corrosion resistance
DUPLEX1.4462X2CrNiMoN22-5-32205S31803≤0,03≤1,00≤2,00≤0,035≤0,01521,0-23,04,50-6,502,50-3,50//0,10-0,22Good resistance to stress corrosion cracking
NON-ALLOY STRUCTURAL STEEL1.0038S235JR+N≤0,20≤1,40≤0,035≤0,035≤0,55
NON-ALLOY STRUCTURAL STEEL1.0577S355J2+N≤0,22≤0,55≤1,60≤0,025≤0,025≤0,55
NON-ALLOY STRUCTURAL STEEL1.0425P265GH≤0,20≤0,400,80-1,40≤0,025≤0,010≤0,30≤0,30≤0,08≤0,03≤0,30≤0,012
NON-ALLOY STRUCTURAL STEEL1.0460P250GH0,18-0,23≤0,400,30-0,90≤0,025≤0,015≤0,30≤0,03
Source: EN10028-7, EN10088, EN10095, EN10025-2, EN10028-2, EN10273